Description & applications

• Seamless high fill copper coated metal cored wire for gas shielded arc welding

• Single and multiple pass welding of creep resisting steels alloyed with 2.25Cr-1Mo

• Optimal productivity by combining advantages of both seamless and seamed tubular wires

• HDM guaranteed < 4 ml/ 100g deposited metal on the whole parameter box

• No moisture pick up, excellent wire feeding properties, good weldability and low spatter

• Designed for service temperatures up to 550°C

APPLICATIONS

Welding creep-resisting steels of similar composition. Preheat 150-250°C and stress relieving 660 -700°C must be carried out.

Examples

Creep resisting steel EN 10028-2 10 CrMo 9-10

Creep resisting steel EN 10222-2 12 CrMo 9-10

Creep resisting steel ASTM A387gr .21 & 22, A182F22, A217WC9, A234WP22

Creep resisting steel ASTM A199, A200T3b, T4, T21, T22, A213T22

Creep resisting steel ISO/TR 15608: Group 5.2

Classification

AWS A 5.28 EN 12071
E90C-B3 H4 T CrMo2 M M 1 H5

Typical weld metal composition (%)

C Mn Si Cr Mo
0.06 1.1 0.3 2.3 1.0

All weld metal mechanical properties

Rm (MPa) Rp0.2 (MPa) A5 (%) KCV
680 580 21 20°C: 90 J PWHT 1h/690°C

Shielding gas

M21 gas mixtures (Ar + 5 - 25% CO2) according to EN 439 / ISO 14175 Gas flow rate: 12 - 25 l/min

Operating conditions

Diameter [mm] Current type Current I [A] Stick out [mm] Voltage [V]
1.2 DC(+) or pulsed 100-350 12-25 15-35
1.4 DC(+) or pulsed 120-400 12-25 15-35
1.6 DC(+) or pulsed 130-450 15-25 15-35

Welding positions

FCW M CrMo2 is primarily used in the flat and horizontal-vertical positions. However, welds in other positions are also possible using the short-circuiting or pulsed arc modes of transfer.

Packings & Diameters

Diameters [mm] 1.2 - 1.4 - 1.6
Packing(s) Spool BS300
Weight [Kg] 15
Description -