High temperature stainless steel electrode
Basic coated austenitic stainless steel electrode with 26%Cr, 35%Ni, 1.2%Nb and an increased carbon contend. Used to weld austenitic heat resistant alloys, centrifugally cast tubes etc. resisting to scaling and oxidation up to 1200°C. Regular and stable fusion, good slag removal, nice aspect of the bead.
Main applications:
Petrochemical industry, for welding centrifugally cast pyrolysist coils, reformer tubes, piping systems.
UNS |
Alloy |
EN |
Material N° |
J93503 |
|
G-X40CrNiSi25 12 |
1.4837 |
J94204 |
HK40 |
G-X40CrNiSi25 20 |
1.4848 |
N08705 |
HP45 |
G-X40NiCrSi35 25 |
1.4857 |
|
|
G-X40NiCr38 18 |
1.4849 |
|
|
G-X40NiCrNb35 25 |
1.4852 |
EN ISO 3581A |
---|
E Z 25 35 Nb H B 4 2 |
C | Si | Mn | Cr | Ni | Nb | Fe |
---|---|---|---|---|---|---|
0.4 | 1.0 | 1.8 | 26.0 | 35 | 1.2 | Base |
Rm MPa | Rp0,2 MPa | A 5(%) |
---|---|---|
> 660 | > 440 | > 12 |
Dimension | 2.5x300 | 3.2x350 | 4.0x350 |
---|---|---|---|
Electr. / packet | 211 | 139 | 94 |
Electr. / carton | 844 | 556 | 376 |
Kg 1000 electr. | 19 | 36 | 53 |
Packets / carton | 4 | 4 | 4 |
Kg / packet | 4 | 5 | 5 |
Kg / carton | 16 | 20 | 20 |
A | 70 | 100 | 135 |
---|
Redrying 2 hours at 250°C, if necessary. Interpass temperature: <150°C.
= +