Abranel 1S

Basic coated NiCrMo electrode highly corrosion resistant

Description & applications

Rutil-basic coated electrode with high recovery (170%) for welding of Nickel-Chromium-Molybdenum alloys to themselves and to lower alloyed steels as well as for welding of special austenitic stainless steels. For butt-welding and surfacing on low alloyed and high strength steels as well as for dissimilar joints and buffer layers. Crack resistant buffer layers on machine parts in earth movement and steel-industries subject to impact and pressure.

Uns Nr : K 81340, N08926, N08825, N06625

DIN design : X8Ni9 - X1NiCrMoCuN25 20 6 - NiCr21Mo - NiCr22Mo9Nb

Mat n° : 1.5656 - 1.4529 - 2.4858 - 2.4856

Classification

AWS A5.11 UNS EN ISO 14172
E NiCrMo-3 W86112 E-Ni6625 NiCr22Mo9Nb

Typical weld metal composition (%)

C Si Mn Cr Mo Fe Nb Ni
0.04 0.5 0.8 21.0 8.5 4.0 3.3 Rest

All weld metal mechanical properties

Rm (MPa) Rp0.2 (MPa) A5 (%) Hardness
>760 >450 >30 ~240 HB

Packaging data

Dimension 2.5x350 3.2x350 4.0x350
Electr. / packet 160 94 61
Electr. / carton 640 376 244
Kg 1000 electr. 31.2 53 82
Packets / carton 4 4 4
Kg / packet 5 5 5
Kg / carton 20 20 20

Amperes

A 70-90 90-120 120-140

Welding Instructions

Redrying 1 h at 250-300°C. Joints to weld must be clean, exempt from grease, cracks. Guide electrodes with a slight declination, weld with a short arc and prevent a high heat input by applying the stringer bead technique ( weaving max. 2 times core wire diameter ). For repair welding a preheating, depending on the carbon equivalent of the base material, in the range of 100-250°C is recommended.

= + ~ 70V