Description & applications

• Seamless high fill copper coated basic cored tubular wire for semi-automatic gas shielded arc welding

• 1 % nickel alloyed to improve sub-zero impact strength

• Single and multipass welding of cold tough / fine-grained steels

• Optimal productivity by combining advantages of both seamless and seamed tubular wires

• HDM guaranteed < 4 ml/ 100g deposited metal on the whole parameter box

• No moisture pick up, excellent wire feeding properties, good weldability and low spatter

APPLICATIONS

Fine-grained, cold tough (down to -60°) and high yield strength steels (up to 550 MPa)

Examples

Construction steels EN 10025 S235JR to S355K2G4

Fine-grained steels EN 10028-3 P275N, NH, NL1, NL2 to P460N, NH, NL1, NL2

Fine-grained steels EN 10113 S275N to S460N, S275M to S460ML

Pressure vessel steels EN 10028-2 P235GH to P355GH

Pipe steels EN 10208 L240NB to L445NB API 5LX X42, X46, X 52, X60, X65

Shipbuilding steels A, B, D, E, A32/36 to F40

Shipbuilding steels ISO/TR 15608: Groups 1.1, 1.2, 1.3, 2.1 and 3.1

Classification

EN ISO 17632-B EN ISO 17632-A AWS A 5.29
T556T5-0MA-N3-H5 T 46 6 1Ni B M 3 H5 E80T5-G H4

Typical weld metal composition (%)

C Mn Si Ni
0.06 1.4 0.4 1.1

All weld metal mechanical properties

Rm (MPa) Rp0.2 (MPa) A5 (%) KCV
600 520 24 -60°C : 80 J

Shielding gas

M21 gas mixtures (Ar + 5 - 25% CO2) according to EN 439 / ISO 14175 Gas flow rate: 12 - 25 l/min

Operating conditions

Diameter [mm] Current type Current I [A] Voltage [V] Stick out [mm]
1.2 DC(+) or pulsed 110-350 16-34 12-25
1.4 DC(+) or pulsed 130-370 16-34 12-25
1.6 DC(+) or pulsed 160-470 20-36 15-25
2.4 DC(+) or pulsed 300-550 30-36 15-25

Welding positions

EN ISO 6947: PA, PB, (PF, PC – Ø 1.2 mm)

ASME IX: 1G, 1F, 2F, 3Gu, 2G – Ø 1.2 mm)

Packings & Diameters

Diameters [mm] 1.2 - 1.4 - 1.6 - 2.4
Packing(s) Spool BS300
Weight [Kg] 15